Description
NiAl 80/20 can be used as an adhesive coating and require minimal surface treatment. Bond strengths in excess of 9000 psi can be obtained on blasting surfaces of gravel. It has good resistance to high temperature oxidation and abrasion, and excellent resistance to impact and bending.
For arc and flame spraying systems
Bond coats
High temperature corrosion protection
C | Si | S | Mn | Cr | Ni | Al | P |
≤0.08 | 0.75-1.6 | ≤0.015 | ≤0.6 | 20.0-23.0 | Bal. | ≤0.5 | ≤0.02 |
Typical Hardness HRB | Bond Strength PSI | Deposit Rate lbs /hr/100A | Deposit Efficiency | Machilityineab |
60-75 | 9100 | 10 | 60-70% | Good |