Hastelloy˘ C-276 Available in any of the 'profile options' This Nickel-Molybdenum-Chromium alloy with the addition of Tungsten, has excellent corrosion resistance in a wide range of corrosive media and is especially resistant to pitting and crevice corrosion.
Made In China Low Price ERNiCrMo-3 Wire For Welding Equivalent To Inconel 625
Hastelloy˘ C-276
Available in any of the 'profile options'
This Nickel-Molybdenum-Chromium alloy with the addition of Tungsten, has excellent corrosion resistance in a wide range of corrosive media and is especially resistant to pitting and crevice corrosion.
Chemical Composition | Specifications | Designations | Key Features | Typical Applications |
---|---|---|---|---|
ElementMin %Max %Mo15.0017.00Cr14.5016.50Fe4.007.00W3.004.50Co-2.50C-0.01Si-0.08Mn-1.00V-0.35P-0.04S-0.03Nibal | ASTM B574 ASTM B575 ASTM B619 ISO 15156-3 (NACE MR 0175) | W.Nr 2.4819 UNS N10276 AWS 054 | Excellent corrosion resistance in a wide range of corrosive media including, sulphur compounds and chloride ions Excellent resistance to pitting, crevice corrosion and stress corrosion cracking Withstands the corrosive effects of wet chlorine gas, hypochlorite and chlorine dioxide Good for sea water applications. | Pollution control Chemical processing Waste treatment Marine engineering Pulp and paper production |
Density | 8.89 g/cm³ | 0.321 lb/in³ |
Melting Point | 1370°C | 2500°F |
Coefficient of Expansion | 11.2 μm/m °C (20 - 100°C) | 6.2 x 10-6 in/in °F (70 - 212°F) |
Modulus of Rigidity | 78.6 kN/mm² | 11400 ksi |
Modulus of Elasticity | 205.5 kN/mm² | 29806 ksi |
Heat Treatment of Finished Parts | |||||
---|---|---|---|---|---|
Condition as supplied by Alloy Wire | Type | Temperature | Time (Hr) | Cooling | |
°C | °F | ||||
Annealed or Spring Temper | Stress Relieve | 400 - 450 | 750 - 840 | 2 | Air |
Properties | ||||
---|---|---|---|---|
Condition | Approx. tensile strength | Approx. operating temperature | ||
N/mm² | ksi | °C | °F | |
Annealed | 850 - 1050 | 123 - 152 | -200 to +400 | -330 to +750 |
Spring Temper | 1300 - 1600 | 189 - 232 | -200 to +400 | -330 to +750 |
The above tensile strength ranges are typical. If you require different please ask.