Superalloy Uns N07090 Ws 2.4632 Nicr20co18ti Round Bar
Description
UNS N07090,Werkstoff Nr. 2.4632,Werkstoff Br. 2.4969,NiCr20Co18Ti,NCK20TA (AIR 9165),BS HR2,AMS 5829,MSRR 7137, MSRR 7017,GH90(China)
It mainly used for turbine engine combustor components operating below 800ºC and other high temperature components requiring oxidation resistance but low load below 1100ºC,such as combustion chambers and afterburners and the mounting edge of the casing.
Superalloy Uns N07090 Ws 2.4632 Nicr20co18ti Round Bar
Common specification in different countries:
UNS N07090,Werkstoff Nr. 2.4632,Werkstoff Br. 2.4969,NiCr20Co18Ti,NCK20TA (AIR 9165),BS HR2,AMS 5829,MSRR 7137, MSRR 7017,GH90(China)
Nimonic alloys are primarily composed of nickel and chromium.These alloys are known for their high-temperature low-creep and high performance. Additives like aluminium, carbon and titanium are infused into the alloy. The Nimonic alloy was first developed in 1940 in England.
Nimonic 90 characteristics:
As high temperature alloy,because it does not have a sensitization tendency after 50 hours of incubation at ultra-high temperature.
As corrosion resistant alloy,because it has better corrosion resistance invarious oxidizing and reducing environments.
As wrought alloy, because the alloy can be hot and cold deformed.
As casting alloy,because the alloy can be used to make certain parts that can only be formed by casting.
Nimonic 90 Chemical Content:
Alloy
Cr
Co
Al
Ti
Ni
C
Mn
Si
P
S
Cu
Fe
Zr
Nimonic 90
18.0-21.0
15.0-21.0
1.0-2.0
2.0-3.0
Bal.
≤0.13
≤0.4
≤0.8
≤0.02
≤0.015
≤0.2
≤1.5
≤0.15
Nimonic 80A Physical Properties:
Density(g/cm3)
8.2
Melting point(ºC)
1400
Application: Ni-Cr alloy is also a nickel-based heat-resistant alloy; it is mainly used under oxidizing medium conditions. These alloys also have good resistance to hydroxide (such as NaOH, KOH) corrosion and stress corrosion resistance. Ni-Mo alloy is mainly used under the condition of reducing medium corrosion. It is an alloy that is resistant to corrosion, but in the presence of oxygen and oxidants, the corrosion resistance decreases significantly. Nimonic90 Ni-Cr-Mo,this alloy combines the properties of the Ni-Cr alloy and Ni-Mo alloy. It is mainly used under the condition of oxidation-reduction mixed medium. Such as: 1.Ocean: marine structures in the sea environment, seawater desalination, seawater aquaculture, seawater heat exchange, etc. 2. Environmental protection field: flue gas removal device for thermal power generation, wastewater treatment, etc. 3. Energy field: atomic power generation, comprehensive utilization of coal, sea tide power generation, etc. 4. Petrochemical industry: oil refining, chemical and chemical equipment, etc. 5. Food field: salt making, soy sauce brewing, etc.
In the form of:
Nimonic 90 are mainly available in sheet, strip, plate, bar, wire, tube.