Superalloy Ni-Cr Based Alloy Gh3030 Round Bar

Description

GH3030, solid solution strengthened superalloy with simple chemical composition, satisfactory thermal strength and high plasticity below 800ºC, and good performance in oxidation resistance, thermal fatigue, cold stamping and welding process. It is monocrystalline austenite structure after solution treatment, and the structure is stable during use. It mainly used for turbine engine combustor components operating below 800ºC and other high temperature components requiring oxidation resistance but low load below 1100ºC,such as combustion chambers and afterburners and the mounting edge of the casing.

Content_1

Content_2

ProInfoAttach

ProDetailSubTitle2

Superalloy Ni-Cr Based Alloy Gh3030 Round Bar


(Common Name: GH30, ЭИ435, XH78T)


GH3030, solid solution strengthened superalloy with simple chemical composition, satisfactory thermal strength and high plasticity below 800, and good performance in oxidation resistance, thermal fatigue, cold stamping and welding process. It is monocrystalline austenite structure after solution treatment, and the structure is stable during use.


It mainly used for turbine engine combustor components operating below 800 and other high temperature components requiring oxidation resistance but low load below 1100,such as combustion chambers and afterburners and the mounting edge of the casing.

Normal composition%

CCrNiTiAlFeMnSiPSCu
≤0.1219.0-22.0Bal.0.15-0.35≤0.15≤1.5≤0.7≤0.8≤0.02≤0.02≤0.20

Typical Mechanical properties

Tensile StrengthElongation
Mpa%
785≥25

Typical Physical properties

Density (g/cm3)8.4
Electrical resistivity at 20ºC(10-6ohm.m)1.09
Conductivity coefficient at 100ºC (λ/(W/(m·ºC))15.1
Specific heat capacity at 150ºC(J/(kg·ºC))565.2
Magnetic properties  None